Detail Information |
|||
Model Number: | CC40 | Available Color: | 10 Standard Colors |
---|---|---|---|
Raw Materila: | Everflon Virgin FEP Add Pigment | Pigment Content: | 12% |
Addtive Rate: | 1-3% | Supply Ability: | 1000 Kilogram/Kilograms Per Month |
High Light: | polymer masterbatch,pigment masterbatch,etfe cc40 color concentrate |
Product Description
Color Masterbatch/ ETFE Color Concentrate / Virgin Pellets / 10 Standard Color Supply
Brief Introduction
Everflon® ETFE CC40 color concentrate is compound of color pigment and everflon ETFE virgin resin could be additive with Everflon ETFE virgin pellets to produce color ETFE products by extrusion, injection and molding processing method.
Everflon® ETFE PC40 pre-colored pellets is compound between color concentrate and virgin resin, could be processed color products directly with good quality.
We supply ETFE Color Masterbatch
• 10 standard and custom colors;
• metal free content and reach SGS-RoHS certificate;
• could mix with most main brand ETFE materials with excellent disparity
• Pre-colored compounds
Data List of Everflon ETFE Color Masterbatch
ETFE Color Concentrate | ETFE Pre-colored Resins | ||
Color | Grade | Color | Grade |
White | 9003 | White | 22W |
Black | 9017 | Black | 22B |
Red | 3001 | Red | 22R |
Orange | 2000 | Orange | 22O |
Green | 6024 | Green | 22G |
Yellow | 1023 | Yellow | 22Y |
Blue | 5017 | Blue | 22L |
Brown | 8001 | Brown | 22G |
Purple | 4006 | Purple | 22P |
Gray | 7004 | Gray | 22H |
15% pigment inside with Everflon PFA base | 3% Everflon color concentrate inside |
Main Processing Way of Everflon ETFE Color Concentrate
Insulation Thickness | WT% with ETFE Pellets | Percentage% |
0.1-0.15mm | 1:10-20 | 5-10 |
0.2-0.25mm | 1:20-30 | 3-5 |
0.3-0.50mm | 1:30-50 | 2-3 |
Package&Delivery
Everflon® ETFE color masterbatch is packaged in 25kg, single layer, plastic bags. For convenient shipment, orders of 1,000-kg pallets are recommended.
The properties of Everflon® ETFE resins are not affected by storage time. Ambient storage conditions should be designed to avoid airborne contamination and water condensation on the resin when opening and emptying the packaging.